BegoPal 300 - Pd 75.2%

Based alloy for metal-ceramic restorations

  • Wide range of indications – from crowns to superstructures

  • Copper-free – ideal for sensitive patients

  • Light-coloured oxide – greater reliability in the colouring of the ceramic

  • Alloyed with gold and silver – excellent melting, flow and soldering properties

  • Biocompatible and corrosion-resistant

Product details

Composition in % by mass


Pd 75.2 · In 6.3 · Ag 6.2 · Au 6.0 · Ga 6.0 · Re · Ru


Alloy characteristics

Standard values

Type (ISO 22674)

4

BEGO colour code

8

Density

11.0 g/cm3 

Preheating temperature

850 °C 

Solidus, liquidus temperature

1 175, 1 320 °C 

Casting temperature

1 390 °C 

Young's modulus

135 GPa 

Proof strength (Rp0,2)

520 MPa 

Ultimate strength (Rm)

910 MPa 

Elongation after fracture (A 5)

28 %

Vickers hardness

240 HV5

Coefficient of thermal expansion (CTE) 25–500 °C, 10-6 K-1 

13,8

Availability

REF

BegoPal® 300, 25gr* 

61105

Accessories

REF

Laser welding wire :

BegoPal® 300 Ø 0,35 mm

61165

BegoStar® solder before firing

61081

BEGO-GOLD solder after firing

61017

Minoxyd Flux 

52530

*Sold in 25-gram pack. Price per gram fluctuates according to daily market prices.

The BEGO Colour Code

The areas of colours within the characteristic fields approximately correspond to the intensity of the alloy colours.

  • Wide range of indications – from crowns to superstructures

  • Copper-free – ideal for sensitive patients

  • Light-coloured oxide – greater reliability in the colouring of the ceramic

  • Alloyed with gold and silver – excellent melting, flow and soldering properties

  • Biocompatible and corrosion-resistant

Related products

Bego gold solder I

BegoStar solder

Additional materials for laser welding

Information request for the product: 

BegoPal 300 - Pd 75.2%

Province or territory
bottom of page